摘要 |
The invention relates to a stretched polymer film made of a polyamide composition comprising a semi-crystalline semi-aromatic polyamide (PPA), wherein the PPA consists of repeat units derived from aromatic dicarboxylic acid comprising at least 80 mole % of terephthalic acid, relative to the total amount of aromatic dicarboxylic acid; and diamine comprising at least 5 mole % 1,4-butanediamine and at least 5 mole % 1,6-hexanediamine, relative to the total amount of diamine, the combined amount of 1,4-butanediamine and 1,6-hexanediamine being at least 60 mole % relative to the total amount of diamine; and 0-2 mole % of other monomeric units, relative to the total amount of aromatic dicarboxylic acid, diamine and other monomeric units. The invention further relates to a process for preparing the polyamide film by melt extrusion and stretching of the film. |