摘要 |
PURPOSE:To obtain the distinct color print at a low cost, by a method wherein a roughened surface layer and a metal vapor deposited layer are successively installed on a substrate and besides, the roughened surface layer of a transfer medium is let to involve carbon by not less than 10wt%. CONSTITUTION:The roughened surface layer 10 is let to involve carbon 12 by 10wt% min and given semiconductor property. Thereby, the resistant gap between the metal vapor deposited layer 13 and the roughened surface layer 10 is kept suitably. Then, the spark noise generated by discharge recording is eliminated and a sharp distinct printing can be obtained. Furthermore, earthing return can be prevented. When transferred by using the flash of infrared ray, the roughened surface layer 10 is operated as a light and heat convension layer because of carbon involved in the roughened surface layer 10. Therefore, it is not necessary to establish the light and heat conversion layer newly and cost down is obtained. Further, the surface roughness of metal vapor deposited layer 13 is within a range of 5-150sec in Bekk, smoothness and good discharge recording can be carried out. |