摘要 |
<p>As a construction material in sulphurous environments at high temperatures it has according to the invention been found advantageous to use an austenitic chromium-nickel-manganese alloy having a relatively high content of manganese such as 3-12% and preferably 3-8%,
<UnorderedLists id="ula01" listStyle="none"><ListItem>carbon up to 0.5%,</ListItem><ListItem>silicium up to 3.0%,</ListItem><ListItem>chromium 18-30 and</ListItem><ListItem>nickel 11-35%</ListItem></UnorderedLists></p> |