发明名称 Process for producing, by continuous annealing, soft blackplate for surface treatment.
摘要 <p>Steel blackplate for surface treatment, having a soft temper degree of T-3 or less, and improved fluting resistance is produced by the combination of a chemical composition of 0.01 % to 0.08% carbon, 0.015% or less phosphorus, without titanium and niobium; steelmaking without vacuum-degassing; a low slab-heating temperature of 1240°C or less; a coiling temperature of 620°C to 710°C; continuous annealing having a heat pattern to decrease the solute carbon and nitrogen; and skin-pass rolling.</p>
申请公布号 EP0171197(A2) 申请公布日期 1986.02.12
申请号 EP19850304890 申请日期 1985.07.09
申请人 NIPPON STEEL CORPORATION 发明人 MARUOKA, KUNIAKI C/O NIPPON STEEL CORPORATION;TAKAHASHI, NOBUYUKI C/O NIPPON STEEL CORPORATION;TUJIMURA, SENKICHI C/O NIPPON STEEL CORPORATION;YAMASHITA, YASUHIKO C/O NIPPON STEEL CORPORATION;OTSUKA, SETSUO C/O NIPPON STEEL CORPORATION;OOHASI, ISAO C/O NIPPON STEEL CORPORATION;MOTOYAMA, TAKEO C/O NIPPON STEEL CORPORATION
分类号 C21D8/02;C21D9/52;(IPC1-7):C21D8/02 主分类号 C21D8/02
代理机构 代理人
主权项
地址