摘要 |
Coercivity of ferromagnetic particles is increased by depositing multiple layrs containing transition metals, including cobalt, on the surface of the particles at ambient temperature. Thereafter, the particles are heated sufficiently to obtain the desired level of coercivity. Typically, total heating time is five to ten hours. |