发明名称 |
Gas metal arc welding process. |
摘要 |
<p>The gas metal arc welding process of the present invention extends the axial spray metal transfer range with a non rotating arc from 10 to 25 Ibs/hr using an electrode wire diameter between .035 to .052 inches. The process is carried out by maintaining an electrode extension of between 3/4 to 1 1/4 inches with a three component shielding gas mixture consisting essentially of argon and oxygen in combination with carbon dioxide or carbon monoxide in a volume proportion of oxygen 1-2%, carbon dioxide 8-15%, balance argon. The arc voltage is maintained in a range of between 29 and 40 volts.</p> |
申请公布号 |
EP0167163(A1) |
申请公布日期 |
1986.01.08 |
申请号 |
EP19850108288 |
申请日期 |
1985.07.04 |
申请人 |
UNION CARBIDE CORPORATION |
发明人 |
DEVITO, JOSEPH;LYTTLE, KEVIN ARTHUR;SUTTON, RONALD DEAN;WESTENDORF, ALAN JOHN;LARSON, NILS EDWARD;UTTRACHI, GERALD DANIEL |
分类号 |
B23K9/16;B23K9/173;(IPC1-7):B23K9/16 |
主分类号 |
B23K9/16 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|