发明名称 FOERFARANDE FOER FRAMSTAELLNING AV FERROKROM MED LAOG KOLHALT I EN REAKTOR
摘要 Low carbon ferrochromium is produced by (a) charging a tilting rotary reactor with chromium mineral and carbonaceous reductant; (b) heating the charge to at least 1200 deg.C; (c) making successive addns. of solid carbonaceous and oxygen blowing while rotating the reactor in the inclined position to produce a carbon-saturated liq. ferrochromium bath; (d) deslagging and decarburising using an oxygen lance, while the reactor is rotating and inclined, to obtain the desired carbon content of 2-0.2 or even 0.1%; and (e) tapping the reactor. An extra low carbon content of down to 0.020 or even 0.010% can be obtd. by reducing the pressure in the reactor to 0.5-50 (pref. 1-10) torr after step (d) and holding for 5-45 mins. A range of low carbon ferrochromium alloys can be produced, at low cost and high productivity, from low quality minerals and variable quality solid reductants.
申请公布号 FI69488(B) 申请公布日期 1985.10.31
申请号 FI19810003573 申请日期 1981.11.11
申请人 SOCIETE FRANCAISE D'ELECTROMETALLURGIE SOFREM 发明人 BOSCARO LOUIS;MONTANTEME JEAN;BUCHER JEAN-PHILIPPE
分类号 C22C33/04;C22C35/00;(IPC1-7):C22C35/00 主分类号 C22C33/04
代理机构 代理人
主权项
地址