发明名称 FLAME-RETARDANT POLYOLEFIN COMPOSITION
摘要 PURPOSE:The titled composition, obtained by incorporating a silicone rubber having a specific viscosity with hydrotalcite, single crystal fibers having a high strength, e.g. potassium titanate, and a metal soap, capable of exhibiting sufficient flame retardancy, and having improved nondripping and mechanical characteristics. CONSTITUTION:A flame-retardant polyolefin composition obtained by incorporating 100pts.wt. polyolefin with 1-10pts.wt., preferably 1-5pts.wt. silicon rubber having 500,000-2,000,000cP viscosity, 10-60pts.wt., preferably 10-30pts.wt. hydrotalcite, 1-20pts.wt., preferably 5-10pts.wt. single crystal fibers having a high strength, about 20mum average fiber length, 0.2-0.3mum average fiber diameter and a diameter and length of 1/50-1/100 those of the conventional glass short fibers and 1-10pts.wt., preferably 3-5pts.wt. metal soap.
申请公布号 JPS60177045(A) 申请公布日期 1985.09.11
申请号 JP19840030914 申请日期 1984.02.21
申请人 SHOWA DENSEN DENRAN KK 发明人 ITOU KAZUMI;HANAI SETSU
分类号 C08K3/26;C08K5/09;C08K7/00;C08K7/08;C08K13/04;C08L1/00;C08L7/00;C08L21/00;C08L23/00;C08L23/02;C08L27/00;C08L33/00;C08L33/02;C08L83/00;C08L87/00;C08L101/00;H01B3/44 主分类号 C08K3/26
代理机构 代理人
主权项
地址