Epoxy resin modified polyether polyols from mixed initiators. |
摘要 |
<p>Modified polyether polyols are made by first optionally alkoxylating, subsequent reaction with epoxy resins and final alkoxylation of mixtures of initiators comprising 60 to 90 weight % of a partially alkoxylated trifunctional initiator and 10 to 40 weight % of a secondary partially alkoxylated initiator having an active hydrogen functionality of from 4 to 8. Preferably, the alkylene oxide component is a blend of ethylene oxide and propylene oxide, and the resulting modified polyol molecules have 0.25 to 2.5 weight % of internally located epoxy resin. Flexible polyurethane foams made from these polyether polyols have improved load bearing properties as compared with those made from prior art polyols. </p> |
申请公布号 |
EP0153821(A2) |
申请公布日期 |
1985.09.04 |
申请号 |
EP19850300768 |
申请日期 |
1985.02.05 |
申请人 |
TEXACO DEVELOPMENT CORPORATION |
发明人 |
CUSCURIDA, MICHAEL;PETERSON, BRUCE WILLIAM |
分类号 |
C08G18/00;C08G18/48;C08G18/58;C08G59/14;C08G65/26;C08G65/28;C08G65/32;C08L63/00 |
主分类号 |
C08G18/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|