发明名称 High-tension high-toughness steel having excellent resistance to delayed fracture and method for producing the same
摘要 A high-tension high-toughness steel excellent in resistance to delayed fracture which consists essentially of 0.15 to 0.50% of C, up to 1.50% of Si, 0.20 to 1.50% of Mn, up to 2.00% of Cr, 0.0005 to 0.0030% of B, 0.005 to 0.10% of acid-soluble Al, up to 0.010% of P, up to 0.0020% of N, 0.010 to 0.050% of Ti and the balance iron and inevitable impurities, and has a tempered martensitic structure obtained by quenching and tempering.
申请公布号 US4537644(A) 申请公布日期 1985.08.27
申请号 US19820420685 申请日期 1982.09.21
申请人 NIPPON STEEL CORPORATION 发明人 TOMINAGA, JIRO;YADA, HIROSHI;HONDA, MITSUO
分类号 C22C38/00;C21D6/00;C22C38/28;C22C38/32;(IPC1-7):C22C38/14 主分类号 C22C38/00
代理机构 代理人
主权项
地址