发明名称 Legierung und deren Verwendung
摘要 <p>An alloy having improved creep resistance and oxidation resistance in the as-cast state contains about 0.35% to 0.75% carbon, about 0.2% to 2% manganese, up to about 2% silicon, about 40% to 55% nickel, about 22% to 33% chromium, about 4% to 6% tungsten, about 2% to 6.5% cobalt, and the balance iron and usual impurities. A preferred composition is carbon 0.45% manganese 1.25% silicon 0.75% nickel 48% chromium 27% tungsten 5% cobalt 3%, balance iron. The alloy is particularly used for furnace components such as radiant tubes and shafts, gas turbines, jet engines, crucibles, internal combustion engines and turbo superchargers.</p>
申请公布号 CH501733(A) 申请公布日期 1971.01.15
申请号 CH19670011209 申请日期 1967.08.09
申请人 BLAW-KNOX COMPANY 发明人 H. ENGLISH,RAY;N. ORNITZ,MARTIN
分类号 C22C19/05;(IPC1-7):C22C39/00;F27D23/00 主分类号 C22C19/05