发明名称 METHOD FOR REMOVING SCALE OF HOT ROLLED STEEL STRIP COILED AT HIGH TEMPERATURE
摘要 PURPOSE:To reduce the consumption of acid in a succeeding pickling stage and to improve the consumption unit of acid, by water cooling a hot rolled steel strip coiled at a specific temperature, before descaling it by providing a bend- stretching and a brushing treatment to it. CONSTITUTION:A coil 2 coiled at 600-700 deg.C after hot rolling, is dipped in the cooling water 3 in a coil-cooling tank 1 by mounting it on a coil-supporting bed 4, and is cooled for about 1-5hr. Next, after taking out the coil 2 from the tank 1 and uncoiling it to bend-stretch, the coil 2 is passed through plural bending rolls 6 arranged zigzag and is brushed by passing it between brushing rolls 7 and holding rolls 8, and finally it is sent to a pickling tank. In this way, the consumption unit of acid is lowered, and the treatment cost of waste acid, etc. are reduced.
申请公布号 JPS6040611(A) 申请公布日期 1985.03.04
申请号 JP19830147564 申请日期 1983.08.12
申请人 KAWASAKI SEITETSU KK 发明人 TANAKA TOMIO
分类号 B21B45/06;(IPC1-7):B21B45/06 主分类号 B21B45/06
代理机构 代理人
主权项
地址