发明名称 |
PROCEDIMENTO DI ACCOPPIAMENTO TRAPEZZI IN ALLUMINA BETA ALCALINA E IN ALLUMINA ALFA E DISPOSITIVO GENERATORE ELETTROCHIMICO COMPORTANTE LA MESSA DI TALE PROCEDIMENTO |
摘要 |
The alpha alumina part is heated to between 1400 DEG C and 1600 DEG C for 10 to 20 hours in a mass of alkaline carbonate or aluminate. It is then disposed in contact with a blank of the alkaline beta alumina part in a sintering enclosure suitable for establishing an atmosphere which is rich in alkaline metal and in heating this enclosure to between 1600 DEG C and 1700 DEG C for between 30 minutes and 4 hours, so as to sinter the alkaline beta alumina part while effecting the connection thereof to the alpha alumina part. The invention is used in manufacturing sodium-sulphur type electric cells. |
申请公布号 |
IT1064060(B) |
申请公布日期 |
1985.02.18 |
申请号 |
IT19760024837 |
申请日期 |
1976.06.30 |
申请人 |
COMPAGNIE GENERALE D ELECTRICITE |
发明人 |
|
分类号 |
C04B35/113;C04B35/64;C04B37/00;H01M2/16;H01M10/39;(IPC1-7):H01M/ |
主分类号 |
C04B35/113 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|