摘要 |
<p>PCT No. PCT/GB81/00169 Sec. 371 Date Mar. 5, 1982 Sec. 102(e) Date Mar. 5, 1982 PCT Filed Aug. 27, 1981 PCT Pub. No. WO82/00785 PCT Pub. Date Mar. 18, 1982.A method of forming a smooth shoulder (16, 14b, 19b), neck (17, 37) and flange (18, 38) at the open end of the cylindrical side wall (12) of a can body (10) comprises the steps of forcing a marginal edge portion (13) of the side wall into at least a first die to form a first portion of reduced diameter having a first shoulder portion (14) and a first cylindrical portion (15); and optionally applying at least one rolling operation to the first portion of reduced diameter, and any further die formed portions of reduced diameter subsequently formed, to generate a smooth shoulder (16, 14, 19b), neck (17, 37) and flange (18, 38). Reference is made to the roll forming process described and claimed in British Pat. No. 1,534,716 as being particularly suitable. The margin-portion (13) is preferably thicker than the rest of the side wall (12).</p> |