摘要 |
PURPOSE:To obtain crystalline iron silicate suitable for a catalyst for Fischer- Tropsch synthesis (having excellent controllability of carbon distribution of product and high activity), by using simultaneously a Fa(II) compd. and a Fe(III) compd. as an iron-supplying source, and carrying out a hydrothermal synthetic reaction. CONSTITUTION:A mixture of a Fe(II) compd. (e.g. ferrous sulfate) and Fe(III) compd. (e.g. ferric sulfate), whose molar ratio [Fe(II)/Fe(III)] is about 0.01-10 is used as an iron-supplying source. And a mixture having a prescribed ratio of a silica source (e.g. silica sol), above-described iron-supplying source, an alkali- metallic ion source (e.g. sodium oxide in water glass) and a reaction auxiliary (tetraalkylammonium bromide) is allowed to react at about 90-200 deg.C and for about 10-200hr. After a solid substance is separated from an aqueous solution, washed with water and dried, it is calcined under an atmosphere at about 300- 900 deg.C and for about 1-100hr to obtain crystalline iron silicate. |