发明名称 |
ANVENDNING AV EN KOPPARLEDNING FOR STRENGGJUTNINGSKOKILLER |
摘要 |
The material consists of a copper alloy containing from 1.5% to 4% of iron and up to 0.04% of a deoxidant. Advantageously, said alloy contains from 2% to 2.5% of iron, from 0.005% to 0.02% of phosphorus as a deoxidant and from 0.05% to 0.25% of zirconium. In addition, the material may be age-hardened. |
申请公布号 |
SE433455(B) |
申请公布日期 |
1984.05.28 |
申请号 |
SE19770008919 |
申请日期 |
1977.08.05 |
申请人 |
KABEL- UND METALLWERKE GUTEHOFFNUNGSHUTTE AG |
发明人 |
H-J * WALLBAUM;H * GRAVEMANN |
分类号 |
B22D11/04;B22D11/059;C22C9/00;(IPC1-7):22D11/04;22C9/00 |
主分类号 |
B22D11/04 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|