发明名称 METHOD AND ALLOY FOR INTRODUCING MACHINABILITY INCREASING INGREDIENTS TO STEEL
摘要 Lead, bismuth and tellurium and/or sulfur are added to steel, to increase the machinability of the steel, in an addition alloy consisting essentially of 5-40 parts lead, 5-40 parts bismuth, up to 6 parts tellurium and up to 25 parts sulfur. The alloy contains at least one of the group tellurium and sulfur, and the alloy has a melting point of at least about 400 DEG C. (752 DEG F.).
申请公布号 DE3067540(D1) 申请公布日期 1984.05.24
申请号 DE19803067540 申请日期 1980.08.11
申请人 INLAND STEEL COMPANY 发明人 HOLOWATY, MICHAEL O.;BHATTACHARYA, DEBANSHU
分类号 B22D1/00;C22C33/00;C22C33/04;C22C38/00;(IPC1-7):C21C7/00;C22C35/00 主分类号 B22D1/00