发明名称 Method for anodizing aluminum materials and aluminized parts
摘要 Aluminum materials and aluminized parts are oxidatively anodized at a bath temperature of 0 DEG to 15 DEG C. and preferably, 0 DEG to 10 DEG C. to produce an anodized layer of aluminum oxide more than 4 microns thick, which is hard, abrasion-proof and can be stained. The anodizing is bath used while conducting air free of or low in carbon dioxide through the bath. It is free of substances which limit the oxide layer to maximally a thickness of about 1 micron (forming layer) and contains 10 to 500 g trisodium phosphate or tripotassium phosphate per liter. In partially aluminized parts, no destruction of the base material occurs during the aluminizing.
申请公布号 US4439287(A) 申请公布日期 1984.03.27
申请号 US19830480072 申请日期 1983.03.29
申请人 SIEMENS AKTIENGESELLSCHAFT 发明人 BIRKLE, SIEGFRIED;STOGER, KLAUS;DE VRIES, HANS
分类号 C25D11/04;C25D11/06;C25D11/08;(IPC1-7):C25D11/08 主分类号 C25D11/04