<p>Improved method for maximizing jet fuel from shale oil involves hydrotreating the treated oil at a temperature of about 600-650.degree.F in the presence of a catalyst having a relatively low metal content and then hydrotreating the oil at a temperature in excess of about 800.degree.F in the presence of a catalyst having a relatively high metal content. A 480.degree.F minus boiling point fraction fractionated from the foregoing process can meet JP-4 jet fuel specifications. Hydrocracking the 480.degree.F plus boiling point fraction results in substantial additional quantities of jet fuel. AP:dd PL30*</p>
申请公布号
CA1160173(A)
申请公布日期
1984.01.10
申请号
CA19810388975
申请日期
1981.10.29
申请人
SUN TECH, INC.;HYDROCARBON RESEARCH, INC.
发明人
REIF, HENRY E.;MARUHNIC, PETER;CHERVENAK, MICHAEL C.