发明名称 |
Diene-containing rubber compositions having improved green strength |
摘要 |
The invention disclosed herein provides a process for preparing a diene-containing synthetic rubber having improved green strength which includes the steps of charging a reaction vessel with water, an emulsifier, an initiator, an N-(alkoxymethyl)acrylamide monomer and a monomer containing a vinyl group, purging the vessel with an inert gas, charging a diene monomer and an activator to the vessel, polymerizing the monomers to form a copolymer; and, thereafter extracting the copolymer from the vessel and any unreacted monomers. A styrene-butadiene composition containing up to about 10 percent by weight of N-(isobutoxymethyl)acrylamide exhibits better stress-strain properties than a comparable styrene-butadiene rubber without the acrylamide compound.
|
申请公布号 |
US4414359(A) |
申请公布日期 |
1983.11.08 |
申请号 |
US19820342670 |
申请日期 |
1982.01.25 |
申请人 |
THE FIRESTONE TIRE & RUBBER COMPANY |
发明人 |
DOUGHERTY, DAVID J.;GUENESIN, BINNUR;SPIEWAK, JOHN W. |
分类号 |
C08F212/00;C08F236/04;(IPC1-7):C08F220/58 |
主分类号 |
C08F212/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|