发明名称 HOT ROLLING REINFORCING BARS WITH LAYERS OF NICKEL OXIDE AND REFRACTORY MATERIAL
摘要 <p>A method of forming steel reinforcing bars and other bar mill products with a protective coating of nickel to enhance the corrosion resistant characteristics of such bars, such method comprising the steps of forming an elongated steel billet with a generally rectangular cross-section, then electroplating a thin layer of nickel ont? said steel billet, painting the exterior surface of said plated steel billet with a slurry consisting essentially of water and a refractory mortar, arranging a plurality of such steel billets in contiguous relationship in a furnace and heating them to a temperature at which they become malleable (approximately 2150 - 2350 F.), then hot rolling the steel billets to form them into elongated generally round bars. The resulting bars have a lightly adhering nickel oxide film at the surface of the bar; an outer layer of wrought nickel; an intermediate nickel-iron layer metallurigally bonded to the nickel and the steel core; and, a nickel containing ferrous substrate on the outer peripheral surface of the steel core. The refractory mortar coating is usually removed from the billets, prior to the rolling thereof, by suitable descaling equipment.</p>
申请公布号 CA1153331(A) 申请公布日期 1983.09.06
申请号 CA19800357584 申请日期 1980.08.05
申请人 MAXWELL, HERRIS M. 发明人 MAXWELL, HERRIS M.
分类号 B21B9/00;C25D5/48;(IPC1-7):B21B9/00 主分类号 B21B9/00
代理机构 代理人
主权项
地址