A hard magnetic alloy comprises iron, boron, lanthanum, and a lanthanide and is prepared by heating the corresponding amorphous alloy to a temperature from about 850 to 1200 K. in an inert atmosphere until a polycrystalline multiphase alloy with an average grain size not exceeding 400 A is formed.
|