发明名称 ROSTFRITT STAL
摘要 A stainless cast steel of ferrite-austenite two-phase structure having high corrosion fatigue strength and high pitting corrosion resistance containing in terms of % by weight, up to 0.1% C, up to 2.0% Si, up to 2.0% Mn, 22.0-27.0% Cr, 5.0-9.0% Ni, 1.1-2.5% Mo, 0.5-2.5% Cu, 0.5-2.0% Co and 0.5-2.0% V, the steel further containing, if desired, one or more kinds of 0.5-2.0% Nb and/or Ta and 0.01-0.5% Ti, the balance being substantially Fe and inevitable impurities.
申请公布号 SE8300954(L) 申请公布日期 1983.08.24
申请号 SE19830000954 申请日期 1983.02.22
申请人 KUBOTA LTD 发明人 HIRAISHI H;NISHIHARA H;SHIOKAWA H
分类号 D21F3/10;C22C38/00;C22C38/42;C22C38/44;C22C38/46;C22C38/52;D21F1/00;(IPC1-7):C22C38/42 主分类号 D21F3/10