摘要 |
<p>These resins are in particular non toxic styrene, acrylic or epoxy resins, with strong cholesterol-decreasing properties which have an apparent density in water of 0.18 to 0.20 g of dry material/ml and water absorption capacity of 69 to 73% by weight of the po lymer weight. The process for producing anionic ion exchange resins with strong cholesterol-decreasing properties in which a mixture of monomers containing a critical percentage of cross-linking monomer, consists of polymerising at a low rate so as to give the polymer a critically predetermined and uniformly distributed degree of crosslinkage, corresponding to an apparent density in water of 0.18 to 0.20 of dry material/ml with water absorption capacity of 69 to 73% by weight of the polymer weight, wherein the polymerisation catalyst used in an organic peroxide in a concentration of 0.2 to 3%, and the cross-linking agent used is a divinyl compound in a percentage of 1.5 to 12%, at a polymerisation temperature of 50.degree. to 80.degree.C.</p> |