发明名称 METHOD OF PREPARING CAUSTIC DOLOMITE
摘要 manufacture of building materials. SUBSTANCE: dolomite raw is preliminarily sprinkled with magnesium chloride solution with density 1.2-1.3 g/cu.cm taken in amount 0.5 to 3.0% of the weight of dolomite material, which is then heated 20-100 min to 450-550 C and then 5-25 min to 600-720 C. EFFECT: improved quality of dolomite binder due to intensified baking process and reduced content of free calcium oxide in product due to preliminary sprinkling. 1 tbl, 3 ex
申请公布号 RU2158241(C2) 申请公布日期 2000.10.27
申请号 RU19980100788 申请日期 1998.01.15
申请人 TUT MATERIALOVEDENIJA I EHFFEKTIVNYKH TEKHNOLOGIJ;MO INSTI AOOT 发明人 BIKBAU M.JA.
分类号 C04B9/00;C04B9/02;(IPC1-7):C04B9/00 主分类号 C04B9/00