摘要 |
<p>A method of coating glass containers and a composition for such coating, wherein a one-step application of the coating is effected, with an aqueous mixture of a polyamino-acrylate ester, a cross-linking agent therefor, a wax, and a vinyl amino silane coupling agent applied to the container at a temperature of between about 200 DEG -400 DEG F. upon exit of the containers from an annealing lehr.</p> |