摘要 |
In a process for coating steel strip with zinc - iron alloy in which molten zinc is removed from the strip by directing gas under pressure against the strip, the temperature of the bath is above 900 DEG F, preferably 900 to 950 DEG F. The bath may have a cooled zone, 800 to 860 DEG F, as described in Specification 1,116,221. |