摘要 |
In a method of producing a superconducting Nb3Sn wire which comprises passing a wire or tape of a niobium-base alloy through a molten metal bath containing tin and then heat-treating it to form a Nb3Sn compound layer on the surface of said wire or tape, the improvement wherein said niobium-base alloy is an alloy comprising niobium and 0.1 to 30 atomic percent of hafnium, and said molten metal bath is a molten bath of pure tin or a tin-base alloy consisting of tin, from 0.1 to 70 atomic percent of one element of Group IIIb of the periodic table selected from the group consisting of gallium, indium, and aluminum, and from 0.1 to 70 atomic percent of one element of Group Ib of the periodic table selected from the group consisting of copper and silver, the total amount of the element of Group IIIb and the element of Group Ib not exceeding 70 atomic percent.
|