发明名称
摘要 PCT No. PCT/AU81/00052 Sec. 371 Date Dec. 29, 1981 Sec. 102(e) Date Dec. 29, 1981 PCT Filed May 8, 1981 PCT Pub. No. WO81/03221 PCT Pub. Date Nov. 12, 1981.There is disclosed a method of forming a furnace cooling element involving casting a metal block or plate (10) around one or more elongated metal tubes (11) which have a protective coating applied thereto, and thereafter the, or each, metal tube (11) is explosively expanded by an explosive charge (12) closer to the surrounding material of the metal plate (10). Also disclosed is a method in which the protective coating on the metal tube is replaced by a full length external shroud tube (21) to increase the thermal efficiency of the cooling element, the inner metal cooling tube (20) is explosively expanded by an explosive charge (23) closer to the surrounding shroud tube (21) prior to casting a metal plate or block (28) around the tube combination (20, 21) to minimize the gap (22) between the outside wall of the metal cooling tube (20) and the inside wall of the metal protective shroud tube (21). Following casting the metal plate or block (28), the metal cooling tube (20 ) is again explosively expanded closer to the protective shroud tube (21) by a further explosive charge (23').
申请公布号 JPS57500549(A) 申请公布日期 1982.04.01
申请号 JP19810501525 申请日期 1981.05.08
申请人 发明人
分类号 B22D19/04;B23K20/08;F27B1/24;F27D1/12;F27D9/00 主分类号 B22D19/04
代理机构 代理人
主权项
地址