摘要 |
<P>PROCEDE DE FABRICATION D'UN SUPPORT DE CATALYSEUR CONSTITUE PAR DE L'ALUMINE, DESTINE A LA PURIFICATION DES GAZ D'ECHAPPEMENT DE VEHICULES.</P><P>ON DESHYDRATE DE L'HYDRATE D'ALUMINE, ON LE GRANULE, PUIS ON LE CALCINE ENTRE 150C ET 850C, EN OBTENANT DES PARTICULES D'ALUMINE; ON PURGE ENSUITE CES PARTICULES DANS UNE SOLUTION AQUEUSE DE BASE CAUSTIQUE OU D'HYDRATE DE SODIUM OU UN MELANGE DES DEUX SOUS PRESSION DE VAPEUR ET A UNE TEMPERATURE ENTRE 120C ET 200C, LE TAUX D'ATTRITION DES PARTICULES ETANT MINIMUM POUR UNE CALCINATION ENTRE 150C ET 850C.</P><P>CE PROCEDE PERMET D'OBTENIR UN SUPPORT DE CATALYSEUR DE HAUTE RESISTANCE A L'ATTRITION ET SUPPORTANT BIEN L'ECHAUFFEMENT.</P>
|