摘要 |
A method for prepg. solid fuels comprise (i) mixing low quality anthracite (below 2,500 kcal/kg), lignite (5,000 kcal/kg) or peat (5,000 kcal/kg) as a major constituents with industrywaste-carbides i.e. synthetic-resin-waste-carbides, paper mill sludge carbides, (ii) adding deodorizer i.e. sthylenmonomer or ethyleneglycole and heating for 60-90 mins in the heatingcombustion-furnace (250 deg.C), (iii) heating by hot blast (170-230 deg.C) in the rotary kiln (10) to separate odor and gas from the raw fuels and (iv) moulding by compression.
|