Process for preparing calcium silicate shaped product.
摘要
<p>A calcium silicate shaped product is produced by forming an aqueous slurry of calcium silicate hydrate obtained by reacting a calcareous source with a siliceous source dispersed in water under heating; molding said aqueous slurry and heat-treating said molded product under the condition providing the equations (I) and (II);<MathDetails id="matha01"><MathText><![CDATA[ <img id="ia01" file="imga0001.tif" wi="58" he="5" img-content="math" img-format="tif" inline="no" /> ]]></MathText></MathDetails><MathDetails id="matha02"><MathText><![CDATA[ <img id="ia02" file="imga0002.tif" wi="61" he="5" img-content="math" img-format="tif" inline="no" /> ]]></MathText></MathDetails>wherein ⊖ represents a temperature of the inner part of the molded product (°C) and T represents a time (hour) and providing a percent water loss of the treated molded product of less than 25 wt. %, before drying or steam-curing and drying the molded product.</p>