摘要 |
Contacting deactivated hydrodesulfurization catalyst, such as Co-Mo supported on alumina, with a heteropoly acid, such as molybdophosphoric acid or tungstosilicic acid, in pH range of about 1 to 3 and temperature range of about 20 DEG to 80 DEG C., results, before any coke is burned off the catalyst, in selective abstraction of vanadium and nickel, removal of sulfur, increase in surface area, and increase in pore volume of the catalyst. Subsequent cobalt doping of demetallized catalyst followed by calcination promotes decoking, additional sulfur removal and additional increase in surface area and pore volume. The process results in substantially complete regeneration of catalytic activity.
|