发明名称 |
METHOD OF MAKING ANTIFRICTION PRODUCTS |
摘要 |
METHOD OF MAKING ANTIFRICTION PRODUCTS In accordance with the proposed method of making antifriction products, a porous carbon blank is heated up to 1,800 to 2,200.degree.C and impregnated with molten silicon. The impregnation starts at a temperature of 2,100 to 2,200.degree.C for 3 to 5 minutes, then at 1,800 to 2,050.degree.C for 30 to 40 minutes. Thereafter, the blank is cooled down to a temperature of 900 to 800.degree.C at a rate of 30 to 40.degree.C/min, then down to 200 to 150.degree.C at a rate of 50 to 100.degree.C/min. This permits obtaining products with an even phase distribution, whereby their wear resistance and strength are improved. |
申请公布号 |
CA1102185(A) |
申请公布日期 |
1981.06.02 |
申请号 |
CA19780308794 |
申请日期 |
1978.08.04 |
申请人 |
KOSTIKOV, VALERY I.;TARABANOV, ALEXANDER S.;IVANOV, VITALY A.;ZYKOV, ANATOLY M. |
发明人 |
KOSTIKOV, VALERY I.;TARABANOV, ALEXANDER S.;IVANOV, VITALY A.;ZYKOV, ANATOLY M. |
分类号 |
C04B35/52;C04B35/573;C04B41/50;C04B41/87;F16C33/14;F16J15/34 |
主分类号 |
C04B35/52 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|