发明名称 Method of making razor blade strip from austenitic steel
摘要 This invention provides a steel alloy, for use for razor blades, the ranges of composition of which are given in the table below, the first column giving the maximum range for the alloy elements and impurities (the balance being iron), the second column giving a narrower preferred range, whilst the third column gives a particularly advantageous composition: - Maximum Preferred -Element Range Range Example -Ni% 15 to 25 17 to 22 20 -Cr% 3 to 8 3.5 to 5 4 -Ti% 2 to 5* 3 to 4.5 4 -Al% 1 to 5* 2 to 4 3 -C% less than 0.02 0.01 0.005 -Mn% less than 0.2 0.1 0.05 -Si% less than 0.2 0.1 0.05 -N% less than 0.02 0.01 0.003 -P, S% less than 0.02 0.01 0.005 -*but Ti + Al should be less than 9% -
申请公布号 US4259126(A) 申请公布日期 1981.03.31
申请号 US19790075550 申请日期 1979.09.14
申请人 WILKINSON SWORD LIMITED 发明人 COLE, WILLIAM L.;STOTT, GEOFFREY;BOWDEN, HUMPHREY G.
分类号 C21D8/02;C21D9/18;C22C38/50;(IPC1-7):C21D1/20;C21D7/14 主分类号 C21D8/02
代理机构 代理人
主权项
地址