摘要 |
A method of welding at least two layers (18, 20) of thermoplastic material, e.g. polyethylene terephthalate or polyporopylene, and a weld (30) so produced comprises directing a jet of hot gas from a nozzle (10), through a hole (16) in an inlet mask (16), and against the layers (18, 20). The layers (18, 20) are backed by an outlet mask (22) having a hole (26) and serving as a heat sink. The inlet mask (16), the layers (18, 20), and the outlet mask (22) are clamped together. A transverse weld (30) is formed entirely of the material of the layers (18, 20). The weld (30) has a columnar shape with an enlarged end (32 min ), which is cold-headed. The opposite end of the weld is level with or depressed with respect to marginal surfaces of the adjacent layer (18, 20). If the material is crystallizable, the weld may be more crystalline than other portions of the layers. |