发明名称 In situ furnace metal desulfurization/nodularization by high purity magnesium
摘要 A method of desulfurizing iron in an induction furnace is disclosed. High purity magnesium, carried in a lance controlled cartridge, is plunged into the lower zone of a molten metal pool of an induction furnace; the cartridge is held submerged for a period of 30-200 seconds. The molten metal column above the submerged cartridge must be at least 2.5 feet, preferably 6-7 feet. The molten metal temperature at the time of cartridge plunging is limited to 2400 DEG F. or less. Magnesium recovery will be at least 70%, which is better than other prior art methods by a factor of 1.4.
申请公布号 US4204666(A) 申请公布日期 1980.05.27
申请号 US19780943274 申请日期 1978.09.18
申请人 FORD MOTOR 发明人 MOHLA, PREM P
分类号 C21C1/02;C21C1/10;(IPC1-7):C21C1/02;C21C7/02;C22C33/10;D02G3/00 主分类号 C21C1/02