发明名称 |
ZINC SILICATE MINERAL RECOVERING METHOD |
摘要 |
<p>PURPOSE:To advantageously recover zinc silicate mineral of enhanced Zn grade by sulfurizing zinc silicate mineral-contg. ore pulp at a specified temp. and pH followed by flotation. CONSTITUTION:Zinc silicate mineral-contg. ore pulp is sulfurized at 60 deg.C or above and pH 7-9.5, pref. 7.5-9 by adding a sulfurizing agent such as Na2S or NaHS in an amt. of 30kg or more per ton of ore. The sulfurization product is then subjected to flotation. By this method the mineral surface is well sulfurized, so flotation efficiency is enhanced furthermore, and a concentrate of the mineral is obtd. advantageously.</p> |
申请公布号 |
JPS5560018(A) |
申请公布日期 |
1980.05.06 |
申请号 |
JP19780132238 |
申请日期 |
1978.10.27 |
申请人 |
MITSUI MINING & SMELTING CO |
发明人 |
KAHANZAKA JIYUNZOU;MATSUOKA ISAO;OOTAKA KOUICHI;TANABE MITSURU |
分类号 |
C22B19/34;C01B33/20;C01G9/08;C22B19/00;C22B19/20 |
主分类号 |
C22B19/34 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|