发明名称 DAMPING MATERIAL WITH AIRRCRUSHED SLAG
摘要 PURPOSE:To achieve damping effect by mixing the air-crushed slag to the visco- elastic material at the appropriate rate. CONSTITUTION:65 Capacity % air-crushed slag of more than 100mu grain size is mixed into the visco-elastic materials cush as epoxy resin, unsaturated polyvynyl chloride resin, rubber chloride, polyehylene resin, or polypropylene chlorine resin to make the damping member material. The hollow part 1, connected with outside, of the grain shaped slag obtained by crushing the slag, by wind, which is generated by operating metal smelting furnace such as the revolving furnace or the blast furnace has the damping effect against the visco-elastic substances.
申请公布号 JPS5540303(A) 申请公布日期 1980.03.21
申请号 JP19780110624 申请日期 1978.09.11
申请人 NIPPON KOKAN KK 发明人 TAKAKU HIROSHI;TANABE SHIYUUGO;IKEUCHI KOUTAKA;MIZUNO KAZUJI
分类号 C08K3/00;C08K3/34;C08L1/00;C08L7/00;C08L21/00;C08L23/00;C08L27/00;C08L67/00;C08L101/00;F16F9/00;F16F15/02 主分类号 C08K3/00