摘要 |
A molding composition of improved toughness, thermal stability, flow and stress craze resistance comprising (A) from about 70 to about 95% of a resinous terpolymer of 65 to 75 parts of methylmethacrylate, 18 to 24 parts of styrene and 2 to 12 parts of ethylacrylate and (B) 5% to 30% of polybutadiene grafted with 17 to 22 parts of methylmethacrylate, 4 to 7 parts of styrene and 0 to 3 parts of ethylacrylate, the ratio of polybutadiene to monomer in (B) ranging from 1:1 to 4:1, respectively. |