发明名称 |
METHOD FOR PRODUCING TEXTURIZED SILICON STEEL CONTAINING BORON |
摘要 |
A process for producing electromagnetic silicon steel having a cube-on-edge orientation. The process includes the steps of: preparing a melt of silicon steel containing from 0.02 to 0.06% carbon, from 0.0006 to 0.0080% boron, up to 0.0100% nitrogen and from 2.5 to 4.0% silicon; casting said steel; hot rolling said steel; cold rolling said steel; decarburizing said steel to a carbon level below 0.02% in a hydrogen-bearing atmosphere havng a dew point of from +20 DEG F to +60 DEG F; and final texture annealing said steel. |
申请公布号 |
HU173793(B) |
申请公布日期 |
1979.08.28 |
申请号 |
HU1976AE00465 |
申请日期 |
1976.05.14 |
申请人 |
ALLEGHENY LUDLUM INDUSTRIES INC,US |
发明人 |
MALAGARI,FRANK A.,US |
分类号 |
C22C38/00;C21D3/04;C21D8/12;C22C38/02;H01F1/16 |
主分类号 |
C22C38/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|