发明名称 |
CARBOTHERMICALLY PRODUCING ALUMINUM-SILICON ALLOYS |
摘要 |
Aluminum-silicon alloys are formed by bringing a mix containing sources of alumina, silica and carbon to a temperature in the range of 1500 to 1600.degree.C to form silicon carbide and carbon monoxide. The mix containing the silicon carbide is then brought to a temperature in the range of 1600 to 1900.degree.C to form aluminum oxycarbide and carbon monoxide. Thereafter, the mix containing the silicon carbide and aluminum oxycarbide is brought to a temperature in the range of 1950 to 2200.degree.C to produce an aluminumsilicon alloy. |
申请公布号 |
AU2704377(A) |
申请公布日期 |
1979.01.18 |
申请号 |
AU19770027043 |
申请日期 |
1977.07.15 |
申请人 |
ALUMINIUM CO. OF AMERICA |
发明人 |
CHARLES NORMAN COCHRAN;SUBODH KUMAR DAS;RICHARD ALDO MILITO |
分类号 |
C22B4/06;C22B21/02;C22C1/02 |
主分类号 |
C22B4/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|