发明名称 VERFAHREN ZUR BEHANDLUNG VON HOLZSCHNITZELN ZUR SCHNELLEN HARZALTERUNG
摘要 <p>Air is circulated through a body of wood chips at a rate sufficient for maintaining a uniform temperature and oxygen content throughout the body of wood chips. Fresh air is supplied at a rate sufficient for keeping the oxygen content of the circulating air at 16% by volume, at least. The temperature is maintained at 35 DEG -80 DEG C. This process results in a rapid seasoning of the natural resin, of the wood chips, making it possible to use the wood chips for pulping after 1-4 days only.</p>
申请公布号 AT347782(B) 申请公布日期 1979.01.10
申请号 AT19750009334 申请日期 1975.12.09
申请人 BILLERUDS AKTIEBOLAG 发明人 RYHMAN JENS OLOV;VOGT NILS ANTON
分类号 D21C1/00;D21C1/08;(IPC1-7):21C1/00 主分类号 D21C1/00