发明名称 Process for heat-treating the head of railroad rail
摘要 In the process of heat-treating the head of a railroad rail wherein the rail is stressed so that the head forms a convex arc of predetermined height, the arc height is decreased about 14% after about 10% of the rail head has been heated, and then the original arc height is restored when about 40% of the rail head has been heated and then again decreased when about 60% of the rail head has been heated, and then finally the original arc height is again restored while the last 10% of the rail head length is heat treated.
申请公布号 US4099996(A) 申请公布日期 1978.07.11
申请号 US19770801489 申请日期 1977.05.31
申请人 UNITED STATES STEEL CORPORATION 发明人 TOLEIKIS, JR., JOHN
分类号 C21D9/06;(IPC1-7):C21D1/78 主分类号 C21D9/06