发明名称 FORFARANDE VID STRENGGJUTNING AV STAL
摘要 In the continuous casting of steel with an open casting stream between a tundish and a downstream mould (1), a multi-phase mixture of liquid inert gas and a particulate substance is introduced as a layer (7) onto the surface (5) of the molten metal in the mould. Casting powder together with the inert gas as the multi-phase mixture is applied directly to the surface of the molten metal during the coating, at a distance from the casting stream (2), via a common line (6). This distance is greater than half the diameter (8) of coating stream. The wave (9) caused by the casting stream prevents the casting powder from being swept into the liquid casting head (3). <IMAGE>
申请公布号 SE7714350(L) 申请公布日期 1978.06.29
申请号 SE19770014350 申请日期 1977.12.16
申请人 CONCAST AG;BELIPAR SA 发明人 THALMANN A
分类号 B22D11/10;B22D11/108;B22D11/11;(IPC1-7):B22D11/10 主分类号 B22D11/10
代理机构 代理人
主权项
地址