发明名称 Aluminum-nickel-iron alloy electrical conductor
摘要 Aluminum alloy electrical conductors are produced from aluminum base alloys containing from about 0.20 percent to about 1.60 percent by weight nickel, from about 0.30 percent to 1.30 percent iron, optionally up to about 1.00 percent of additional alloying elements, the remainder being aluminum with associated trace elements. The alloy conductors have an electrical conductivity of at least fifty-seven percent (57%), based on the International Annealed Copper Standard (IACS), and improved properties of increased thermal stability, tensile strength, percent ultimate elongation, ductility, fatigue resistance and yield strength as compared to conventional aluminum alloys of similar electrical properties.
申请公布号 US4080223(A) 申请公布日期 1978.03.21
申请号 US19760703389 申请日期 1976.07.08
申请人 SOUTHWIRE COMPANY 发明人 SCHOERNER, ROGER JOHN;CHIA, ENRIQUE C.
分类号 C22C21/00;(IPC1-7):C22F1/04 主分类号 C22C21/00