发明名称 WERKWIJZE VOOR HET VERBETEREN VAN DE SULFIDISCHE EN OXYDISCHE ZUIVERHEID VAN GEDESOXYDEERDE EN/OF MET ONTZWAVELINGSMIDDELEN BEHANDELDE STAAL- SMELTEN.
摘要 <p>The sulphide and oxide contents of molten steel are reduced, where the steel has been deoxidised and/or treated with an agent to remove sulphur. After deoxidn. and/or desulphurisation, the fine suspended particles in the melt are coagulatd and removed by blowing a mineral mixt. of CaO, SiO2 and Al2O3 into the molten steel. The mineral mixt. may also contain MgO and pref. has a m.pt. of 1300-1400 degrees C.; it should only have a low content of iron and manganese oxides. The mixt. is pref. made by melting the constituents, then solidifying and milling to max. size 0.5 mm. Pref. 0.75-2.5 kg of the mixt. is used per tonne of steel, the pref. mixt. contg. 42% CaO, 35% SiO2, 11.5% Al2O3, balance MgO and 3-4% of other constituents. The mixt. is neutral, and coagulates the fine inclusions without detriment to the quality of the steel. The operation can be conducted in a ladle in 4-12 minuts and combined with sulphur removal.</p>
申请公布号 NL7704992(A) 申请公布日期 1978.01.17
申请号 NL19770004992 申请日期 1977.05.06
申请人 KLOECKNER-WERKE A.G. TE DUISBURG, BONDSREPUBLIEK DUITSLAND. 发明人
分类号 C21C7/00;C21C7/06;C21C7/064;C21C7/076;(IPC1-7):21C7/04 主分类号 C21C7/00
代理机构 代理人
主权项
地址