发明名称 |
ANVENDNING AV EN ALUMINIUMLEGERING FOR PLATAR SOM SKALL LACKERAS |
摘要 |
1383895 Aluminium alloy CEGEDUR SOC DE TRANSFORMATION DE L'ALUMINIUM PECHINEY 27 April 1973 [13 Feb 1973] 20280/73 Heading C7A Aluminium alloy of composition:- The alloy may be homogenized for 10-15 hours at 500-550‹C and hot and cold rolled or cooled to ambient temperature reheated and hot and cold rolled or reheated without homogenization hot and cold rolled, annealed for 1 to 2 minutes at 500- 550‹C water or air quenched, stamped, drawn, panel beaten or welded and painted by stoving. The alloy may be used in the manufacture of car body panels. |
申请公布号 |
SE397109(B) |
申请公布日期 |
1977.10.17 |
申请号 |
SE19730005826 |
申请日期 |
1973.04.25 |
申请人 |
* CEGEDUR SOCIETE DE TRANSFORMATION DE L'ALUMINIUM PECHIN;EY |
发明人 |
R * DEVELAY;R * DESCHAMPS;J * PEYRAUD |
分类号 |
C22C21/12;C22C21/04;C22C21/16;(IPC1-7):22C21/12;22C21/16 |
主分类号 |
C22C21/12 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|