发明名称 Sulfuric acid leaching of nickeliferous laterite
摘要 The leaching efficiency of nickeliferous lateritic ore is optimized by scalping the ore to remove a coarse low-nickel fraction and provide a fine nickel-rich fraction which is then high pressure leached in a sulfuric acid solution by controlling the parameters temperature, pulp density, the rate of acid addition, leaching time, agitation rate, etc., whereby a pregnant solution is obtained with the nickel to (Fe+Al+Cr) ratio exceeding about 2.
申请公布号 US4044096(A) 申请公布日期 1977.08.23
申请号 US19750639712 申请日期 1975.12.11
申请人 AMAX INC. 发明人 QUENEAU, PAUL B.;CHOU, EDDIE C.
分类号 C01G53/10;C22B23/00;(IPC1-7):C01G53/10 主分类号 C01G53/10