发明名称 PROCEDIMIENTO PARA LA PREPARACION DE UNA MEZCLA CAUCHOIDE PEGAJOSA.
摘要 <p>Rubber mixtures consisting of (1) 20 - 75 parts of a copolymer containing 60 - 80% by weight of ethylene, 20 - 40% by weight of an alpha -alkene, and 0 - 20% by weight of one or more polyenes and having, in the unvulcanized state, an elongation at rupture of over 800% and a tensile strength of between 10 and 100 kg/cm2; (2) 80 - 25 parts of at least one polymeric material which is a styrene-butadiene copolymer; polybutadiene or polyisoprene; and (3) a tackifier resin and optionally conventional fillers and additives, wherein the mixture of (1), (2) and (3) has an elongation at rupture of at least 800% and a tensile strength of between 1.3 and 50 kg/cm2.</p>
申请公布号 ES447127(A1) 申请公布日期 1977.06.16
申请号 ES19270004471 申请日期 1976.04.17
申请人 STAMICARBON, B. V. 发明人
分类号 C08L7/00;C08L9/00;C08L21/00;C08L23/00;C08L23/16;C08L101/00;(IPC1-7):08L/ 主分类号 C08L7/00